Zone de Texte: WP – Wood Packaging
HT – Heat treatment to at least 56 ºC during at least 30 minutes in the core of the wood
KD – Kiln drying
KD 56 ºC/30 min – The wood is kiln dried and heat treated to at least 56 ºC during at least 30 minutes in the core of the wood. 
DB – debarking 
N.B. This presentation does not cover fumigation, because it is not allowed in Sweden.